Cutback Bitumen Binder: 

 Fm 3 B 2
Fm 2 B 2

Cutback Bitumen Binder:         Fm 2 B 2,      Fm 3 B 2,    Fm 2 B 3,      Fm  2 B 4   

 

 

Cut-back bituminous binder

 

 

 

 

Type : Medium-Curing

 

 

 

 

Grade : Fm 2 B 2

 

 

 

 

Standard : EN 15322

 

 

 

 

 

 

 

 

 

Property                                                     

Test Unit

  Class

Limit

Test Method

Viscosity – Efflux time 4 mm 25 °C

S

Class 2

<200

prEN 12846-2

Solubility

%

Class 2

>99

EN 12592

Flash Point

°C

Class 7

>60

EN ISO 2719

Distillation :

Total distillate to 360 °C

%

Class 7

<55

EN 13358

% of total distillate fraction

 

 

 

 

distilling at 190 °C

%

Class 2

<5

EN 13358

 

 

 

 

 

% of total distillate fraction

 

 

 

 

distilling at 225 °C

%

Class 2

<15

EN 13358

 

 

 

 

 

% of total distillate fraction

 

 

 

 

distilling at 260 °C

%

Class 1

TBR

EN 13358

 

 

 

 

 

% of total distillate fraction

 

 

 

 

distilling at 315 °C

%

Class 1

TBR

EN 13358

 

 

 

 

 

For penetration (after stabilization) at 25 °C ≤ 330x0,1 mm

Stabilization Procedure: EN 13074 -1, followed by EN 13074-2

Penetration at 25 °C

°C

Class 0

NR

EN 1426

 

 

 

 

 

Softening Point,

°C

Class 0

NR

EN 142

 

Cut-back bituminous binder

 

 

 

 

Type : Medium-Curing

 

 

 

 

Grade : Fm 3 B 2

 

 

 

 

Standard : EN 15322

 

 

 

 

 

 

 

 

 

Property                                                     

Test Unit

  Class

Limit

Test Method

Viscosity – Efflux time 4 mm 25 °C

S

Class 3

15-500

prEN 12846-2

Solubility

%

Class 2

>99

EN 12592

Flash Point

°C

Class 6

>65

EN ISO 2719

Distillation :

Total distillate to 360 °C

%

Class 6

<32

EN 13358

% of total distillate fraction

 

 

 

 

distilling at 190 °C

%

Class 2

<5

EN 13358

 

 

 

 

 

% of total distillate fraction

 

 

 

 

distilling at 225 °C

%

Class 2

<15

EN 13358

 

 

 

 

 

% of total distillate fraction

 

 

 

 

distilling at 260 °C

%

Class 1

TBR

EN 13358

 

 

 

 

 

% of total distillate fraction

 

 

 

 

distilling at 315 °C

%

Class 1

TBR

EN 13358

 

 

 

 

 

For penetration (after stabilization) at 25 °C ≤ 330x0,1 mm

Stabilization Procedure: EN 13074 -1, followed by EN 13074-2

Penetration at 25 °C

°C

Class 0

NR

EN 1426

 

 

 

 

 

Softening Point,

°C

Class 0

NR

EN 142

Fm 2 B 3

 

Cut-back bituminous binder

 

 

 

 

Type : Medium-Curing

 

 

 

 

Grade : Fm 2 B 3

 

 

 

 

Standard : EN 15322

 

 

 

 

 

 

 

 

 

Property                                                     

Test Unit

  Class

Limit

Test Method

Viscosity – Efflux time 4 mm 25 °C

S

Class 2

>200

prEN 12846-2

Solubility

%

Class 2

>99

EN 12592

Flash Point

°C

Class 7

>60

EN ISO 2719

Distillation :

Total distillate to 360 °C

%

Class 7

<55

EN 13358

% of total distillate fraction

 

 

 

 

distilling at 190 °C

%

Class 3

<2-5

EN 13358

 

 

 

 

 

% of total distillate fraction

 

 

 

 

distilling at 225 °C

%

Class 3

<10-25

EN 13358

 

 

 

 

 

% of total distillate fraction

 

 

 

 

distilling at 260 °C

%

Class 1

TBR

EN 13358

 

 

 

 

 

% of total distillate fraction

 

 

 

 

distilling at 315 °C

%

Class 1

TBR

EN 13358

 

 

 

 

 

For penetration (after stabilization) at 25 °C ≤ 330x0,1 mm

Stabilization Procedure: EN 13074 -1, followed by EN 13074-2

Penetration at 25 °C

°C

Class 0

NR

EN 1426

 

 

 

 

 

Softening Point,

°C

Class 0

NR

EN 142

Fm 2 B 4

 

Cut-back bituminous binder

 

 

 

 

Type : Medium-Curing

 

 

 

 

Grade : Fm 2 B 4

 

 

 

 

Standard : EN 15322

 

 

 

 

 

 

 

 

 

Property                                                     

Test Unit

  Class

Limit

Test Method

Viscosity – Efflux time 4 mm 25 °C

S

Class 2

>200

prEN 12846-2

Solubility

%

Class 2

>99

EN 12592

Flash Point

°C

Class 7

>60

EN ISO 2719

Distillation :

Total distillate to 360 °C

%

Class 7

<55

EN 13358

% of total distillate fraction

 

 

 

 

distilling at 190 °C

%

Class 3

<2-5

EN 13358

 

 

 

 

 

% of total distillate fraction

 

 

 

 

distilling at 225 °C

%

Class 4

<20-40

EN 13358

 

 

 

 

 

% of total distillate fraction

 

 

 

 

distilling at 260 °C

%

Class 1

TBR

EN 13358

 

 

 

 

 

% of total distillate fraction

 

 

 

 

distilling at 315 °C

%

Class 1

TBR

EN 13358

 

 

 

 

 

For penetration (after stabilization) at 25 °C ≤ 330x0,1 mm

Stabilization Procedure: EN 13074 -1, followed by EN 13074-2

Penetration at 25 °C

°C

Class 0

NR

EN 1426

 

 

 

 

 

Softening Point,

°C

Class 0

NR

EN 142